2006-06-20
11/021,440
2004-12-22
US 7,064,300 B1
2006-06-20
-
-
Tu Hoang
2024-12-22
A method and apparatus achieves making a surface-analysis determination precedent to allowing an electrofusion welding operation on pipe stock which is prescribed to be scraped, skinned or cleaned of surface contaminants prior to being graded ‘passable’ for such electrofusion welding. The method and apparatus utilizes non-contacting probes affixed to the welding power-supply leads such that inspection is automatic on the applicable pipe section(s) contemporaneously prior to enabling power-supply to the hot-wire welding coils. If the applicable pipe section fails the inspection, the welding equipment is disabled until the probes are disassembled, and then re-assembled for a succeeding inspection, such that during the interim an operator presumptively rectifies the situation as by re-scraping or skinning the applicable pipe section.
Get notified when new applications in this technology area are published.
H05B3/58 IPC
Ohmic-resistance heating; Heating elements having the shape of rods or tubes flexible Heating hoses; Heating collars
This application is a continuation of U.S. patent application Ser. No. 10/634,652, filed Aug. 4, 2003 now U.S. Pat. No. 6,858,822, which claims the benefit of U.S. Provisional Application No. 60/400,488, filed Aug. 2, 2002, all of which disclosures are incorporated herein by reference.
The invention relates to electrofusion of thermoplastics and, more particularly, to apparatus and method for making a pipe-surface quality determination preceding electrofusion.
Nowadays thermoplastic fittings are commonly fused or welded to thermoplastic pipes by electrofusion technology. Typically the fitting has an embedded conductor coiled inside it for induction heating by an electrofusion processor to accomplish welding to the pipe. It generally is a prerequisite that the involved pipe surface be cleaned and scraped preceding electrofusion. Scraping importantly accomplishes exposing unvarnished and/or fresh plastic for the electrofusion process. Un-scraped or insufficiently scraped pipe exacerbates problems with achieving leak-tight electrofusion welds. In cases of natural gas piping, leaking natural gas is a tremendous hazard.
To date reliance on whether the pipe is sufficiently scraped preceding electrofusion is reliant wholly on the honesty and/or good judgment of the responsible worker.
It is an object of the invention to provide a machine-controlled determination of pipe surface quality preceding electrofusion of thermoplastics in order to eliminate human error.
A number of additional features and objects will be apparent in connection with the following discussion of preferred embodiments and examples.
There are shown in the drawings certain exemplary embodiments of the invention as presently preferred. It should be understood that the invention is not limited to the embodiments disclosed as examples, and is capable of variation within the scope of the appended claims. In the drawings,
FIG. 1 is an elevational sectional view of two plastic pipe ends butted against one another for permanent joining together by electrofusion technology as known in the prior art, wherein the exterior surfaces of both pipe ends have been cleaned and scraped for a given marginal length extending away from each end such that the scraping exposes unvarnished and/or fresh plastic;
FIGS. 2a, 2b and 2c form a series of views showing an example, prior art, plastic pipe scraper in accordance with U.S. Pat. No. 4,663,794-Evans, which is incorporated by reference, wherein:
FIG. 2a is a side elevational view,
FIG. 2b is a bottom plan view thereof, and
FIG. 2c is a side elevational view comparable to FIG. 2a except showing the scraper in use to accomplish scraping on the exterior of plastic pipe, whereby the scraping process produces a series of spirally formed ridges and valleys proceeding axially along the exterior surface of the pipe;
FIGS. 3a/3b and FIG. 4 form a series of views showing a non-limiting selection of example electrofusion fittings in accordance with the prior art, wherein:
FIG. 3a is a side elevational view of tapping-tee fitting and its mating under saddle, which slides on the lips of the tapping-tee in the direction of the reference arrow until limited by stops,
FIG. 3b is a view in the direction of arrows IIIB—IIIB in FIG. 3a except in the omitting the under saddle, and
FIG. 4 is an elevational sectional view comparable to FIG. 1 except showing an electrofusion coupling fitting slid over the scraped end margins of the abutting pipe ends;
FIG. 5 is a is a side elevational view comparable to FIG. 4 except showing the connection of a pair of probe/connectors in accordance with the invention to the opposite terminals of the electrofusion fitting shown by FIG. 4;
FIG. 6 is an enlarged detail of the right-side probe in FIG. 5 (eg., right relative FIG. 5's perspective) showing a non-contacting probe arrangement in accordance with the invention comprising an emitter (eg., “laser”) and “receiver” for sensing quality of pipe surface matters such as the local presence or absence of sufficient scraping (or skinning) on the pipe exterior;
FIG. 7 is a perspective view of an electrofusion processor modified in accordance with the invention as more particularly described below;
FIG. 8 is a is schematic view of a preferred embodiment of the invention for utilizing the results of surface analysis preceding electrofusion of thermoplastics in accordance with the invention;
FIG. 9 is a flowchart showing a method in accordance with the invention for determining a particular “reference signal” as denominated in FIG. 8;
FIG. 10 is a flowchart showing a method in accordance with the invention for determining passing or failing pipe surface quality preceding electrofusion welding of thermoplastics in accordance with the prior art; and
FIG. 11 is an elevational sectional view comparable to FIG. 4 except showing successful completion of electrofusion welding of the pipe ends and coupling.
The invention relates to apparatus and methods as more particularly described below for making machine-controlled determination(s) of pipe surface quality preceding electrofusion of thermoplastics, and in order to promote elimination of human error.
By way of background, briefly, electrofusion includes at least the practice of mating plastic parts 20 by the fusion achieved from the heat developed in hot-wire coil(s) (eg., 52b in FIG. 4) embedded in one or the other of the parts 50 (eg., typically embedded in a fitting 50, and see FIGS., 3a, 3b and/or 4). FIG. 1 shows the ends 22 of two plastic pipe 20 ends butted against one another in preparation for permanent joining together by electrofusion technology as known in the prior art (although that will require a ‘coupling’ fitting 50 as shown by, eg., as 52 in FIG. 4). The exterior surfaces of both pipe ends 22 have been cleaned and/or scraped (eg., skinned) for a given marginal length 25 extending away from each end 22 such that the scraping (or skinning) exposes newly-exposed plastic. FIGS. 2a, 2b and 2c are a series of views showing an example, prior art, plastic pipe scraper 30 and in accordance with U.S. Pat. No. 4,663,794—Evans.
In general, raw or un-scraped (un-skinned) pipe stock 26 is procured with a varnished or otherwise smooth finish that is unsuitable for electrofusion process(es) while in that raw or un-scraped (un-skinned) condition. That is, there is an unacceptable likelihood that an electrofusion joint will fail quality standards if obtained by plastic parts having any surface varnish or dirt if not oxidation or contamination or OEM printing thereon. Hence it has long been a practice in the industry to scrape off a skin- or surface-layer of the pipe 20 in order to expose fresh or clean plastic 25 which indeed is suitable for electrofusion process(es). Scrapers 30 typically have a blade 32 that is about ⅜-inch (˜10 mm) wide and formed with about twelve shallow teeth 34 across such width such that as a result the scraper 30 might leave about thirty-two lines per inch (−twelve lines per cm) of helically-formed ridges (eg., indicated by reference numeral 40 in FIG. 8, and which are alternated of course by valleys) along the axial extension of the exterior surface of the pipe 20. The prior art scrapers 30 are arranged to auto-advance themselves helically along the axis of the pipe 20 while being turned in complete rotations so that the last furrow left behind by the trailing tooth of the blade 32 plows through the plastic skin more or less accurately parallel and properly spaced relative to the leading furrow cut or plowed one-rotation previously by the leading tooth. In other words, a scraped-section 25 of pipe 20 appears to be formed with a continuous screw thread (eg., as indicated by reference numeral 44 in FIG. 3), having a coarseness at about thirty-two lines per inch (0.8 mm pitch), although relatively finer and much more coarser teeth arrangement are also known in the art.
Additionally, the scraping typically produces a surface roughness of between about 200 micro-inches (˜5/1000ths mm) and 500 micro-inches (˜13/1000ths mm). In contrast, un-scraped sections 26 of the pipe 20 typically exhibit a much smoother finish, measuring for example at about 30 micro-inches (very approximately ˜1/1000ths mm), which despite being smoother is structurally disordered and not nearly as structurally ordered as scraped pipe 25, such structural ordering being (as said) in the form of, eg., screw thread 44.
FIGS. 3a and 3b together show one example of a prior art electrofusion fitting 50, and that being a tapping-tee fitting 51. FIG. 3a shows the tapping tee fitting 51 situated on a section of scraped pipe 25, as prior to electrofusion. FIG. 3a also shows that the tapping-tee fitting 51 has a mating under saddle 51a, which slides on the lips 51b of the tapping-tee 51 in the direction of the reference arrow 51aX until limited by stops. The under saddle 51a is utilized predominantly for temporary clamping purposes only. As soon as the electrofusion weld is completed, the under saddle 51a might be optionally removed as needless although it is typical to leave it in place. If the under saddle 51a were removed after welding, then FIG. 3b shows an axial view (ie., in the direction of arrows IIIB—IIIB in FIG. 3a) of how that would appear.
FIG. 4 shows a further example of an electrofusion fitting 50 in accordance with the prior art, this more particularly being a coupling fitting 52. Coupling fittings 52 receive insertion of the scraped end margins 25 of a pair of abutting pipe ends 22, such as comparably shown previously in FIG. 1. In FIG. 4, the fitting 52 has a barrel section 52a having an inner surface formed with an embedded hot-wire coil conductor 52b wound in a helix around the barrel section 52a and terminating in opposite terminals 52c. To weld, the terminals 52c are connected to connectors “C” (not shown but see, eg., what is denominated as “C” in FIG. 7) of an electrofusion processor (again not shown in this view but see what is denominated as EP100 in, eg., FIG. 7). The electrofusion processor EP100 supplies power to the terminals 52c through the connectors “C.” How much power, and by what profile of power-against-time, is a matter which is highly fitting-specific. Notwithstanding, fitting manufactures widely disseminate such specifications for their fittings 50 and they even code their fittings accordingly, typically by way of a bar code. Prior art electrofusion processors (see for comparison, eg., FIG. 7) include readers of such bar codes by way of for example and without limitation a bar code wand “W” (not shown in FIG. 4 but see, eg., what is denominated as “W” in FIG. 7) in order to search through their memory for what power-against-time profiles are expected, and supply such. The fitting 52 in FIG. 4 furthermore includes a pair of visual ports 52d, which are alongside the pair of terminals 52c respectively. After the fitting 52 has been fused welded to form the pipe connection, the visual ports 52d afford an operator opportunity to visually inspect the success (or not) of the weld. The foregoing are matters of the prior art.
FIG. 5 is a view comparable to FIG. 4 except showing the connection of a pair connectors “C” in accordance with the invention to the pair of opposite terminals 52c of the electrofusion fitting 52 of FIG. 4. The inventive connectors “C” generally combine conventional aspects of supplying power to the terminals 52c along with more particularly a pair of probes 110 in accordance with the invention for making an inventive surface-analysis determination precedent to electrofusion welding.
FIG. 6 shows better one preferred arrangement for the probe(s) 110 in accordance with the invention. The operative principle comprises measuring the reflection, or more accurately the change or loss of such, of an emitted signal as detected or collected by one or more signal receivers 60. Accordingly, the invention preferably operates on the basis of non-contact techniques.
As FIG. 6 more particularly shows, a signal emitter 70 comprises a laser source as, for example and without limitation, a diode laser operating on a six-hundred nanometer wavelength (eg., visible red light). The emission receiver 60 or collector optionally comprises an infrared/photo-transistor although alternatively a photo-diode works as well, and a photo-resistor presents another option still. One such group of usable devices include without limitation CdS cells (and as indicated 62 in FIG. 8).
It is preferred to aim the signal emitter 70 at as shallow angle-of-attack as possible, perpendicular to the ridges 40 of the scraped (or skinned) surface. To date the shallowest angle experimented with has been at 15° although it is believed that, if such can be constructed, half that angle would work better still. FIG. 6 shows that a patch 25p of the scraped surface 24, as illustrated by a dot-dash line, is impinged by the emitted signal. This patch, rather than being an infinitesimally small point, actually has some size. The impinged patch 25p has an ovate shape (if viewed from above) and impinges upon two to five or more lines of ridges 40. Arranging things for a shallower angle is better because correspondingly that means more lines of ridges 40 will obstruct or interfere with the ‘clean’ reflection of the emitted signal.
There are impediments to producing a probe 110 with as shallow angle as desired, and these impediments relate to physical problems when working at such a miniature scale. It is preferred to overcome such impediments by folding the signal with one or more mirrors 81 at least for the purpose of locating both the emitter 70 and collector 60 on the outboard side of the probe 110 where there is more physical space to mount such.
FIG. 7 shows an electrofusion processor EP100 that is modified in accordance with the invention to include circuitry and controls 100 to obtain such functionality as machine-controlled determination of pipe surface quality preceding electrofusion of thermoplastics F100. The electrofusion processor EP100 comprises an input line cord “I,” output leads “O,” output lead connectors “C,” bar-code wand “W,” and various connector adaptors not specifically referenced and partially covered by reference letter “W.” The input line cord “I” plugs into something as public utility power which in this country runs at about one-hundred and twenty VAC line voltage. The electrofusion processor EP100 is configured (or programmed) for stepping through the functions of, among other functions, energizing the probe(s) 110 and analyzing the signal(s) obtained thereby in order to make a quality determination if the pipe surface(s) has(ve) been sufficiently scraped (or skinned or otherwise made suitable). This functionality is more particularly shown in connection with FIGS. 8 and 9. Other functionality which is extra for the purpose includes without limitation data-logging functions F101 which record and store operator functions against a time and date stamp in order to allow ‘ad hoc’ auditing of operator honesty and/or integrity. It is an object of the invention that, in cases of a failing surface-analysis determination, the electrofusion processor EP100 is aborted or disabled A120 from any chance at welding F250 until a passing surface-analysis determination is obtained A125. Presumptively a passing surface-analysis determination A125 can only practicably be obtained by an operator performing a reasonably timely calibration A130 (see FIG. 9) and then, after that, obtaining a very recent passing surface-analysis determination A125 (see FIG. 10) prior to a fusion operation F250. Instances of failing surface-analysis determination to date are presumptively/preferably overcome by an operator (or worker) disassembling the fitting and pipe(s) A135 in order to scrape or re-scrape A140 (skin or re-skin or the like) the involved pipe surface(s) for a succeeding chance to obtain a passing surface-analysis determination A125.
FIG. 8 is a is schematic view of a preferred embodiment of the invention for utilizing the results of surface analysis preceding electrofusion of thermoplastics in order to determine passing or failing surface-analysis determination. The receiver 60 is shown receiving the received signal 83, wherein FIG. 6 shows a preferred arrangement for positioning a signal receiver 60 in accordance with the invention relative to a surface to-be-analyzed and the source 70 of such signal, a signal emitter in accordance with the invention. The receiver 60 provides its own output-signal 85 corresponding to the received signal 83. The receiver's output signal 85 is fed to a comparator 102 (eg., ‘comparison operator’ or like op-amp) which compares the receiver's output signal 85 to a reference signal 87. At present it is preferred if the comparator 102 provides an output which signifies “pass” or “fail” although it is more preferred still if the comparator 102 outputs a range of values corresponding to a range of quality findings (eg., ranging from an upper extreme of fairly superior to a lower extreme of fairly inferior). The output of the comparator 102 is fed to control system 100, as shown generically in FIG. 8. The control system 100 operates to achieve several functions. One, the control system 100 disables the operability of the weld function F250 of the electrofusion processor EP100 until a timely “pass” surface-analysis is achieved. Another, the control system 100 provides a recordable activity F101 for the data-logger to record so that a relatively permanent record is made of the “pass, “fail” and/or ‘degree’ (or other) determination for audit purposes. Additionally, the control system provides the operator with one or more feedback signals so that the operator can act to correct the situation accordingly.
Preferred at present and due to changing preference in the future, it is preferred to compare the received (or measured) signal 83 against a reference signal 87 in order to make a “pass” or “fail” (or in-between quality) surface-analysis determination F100 in accordance with the invention. It is known, however, in fields of industry outside the invention to utilize multiple metrics and/or criteria to make a surface-analysis evaluation, such as disclosed by and without limitation Lasercheck® gauge of the Optical Dimensions Co., of Lake Forest, Calif. Ideally it might be desirable to utilize the most advanced technology available to make a most complete surface-analysis determination. But in the real world of protecting against human error in electrofusion practice it is more realistic to practice technology which is highly competent though not the most advanced for the purposes of making a “pass” or “fail” (or in-between) surface-analysis determination precedent to electrofusion. It is believed that utilizing highly-competent in contrast to the most-advanced technology is more practical when better opportunity for advancing the objects of the invention are to be obtained from analyzing a larger area/circumference of the pipe(s).
FIG. 9 is a flowchart showing a methodology 150 in accordance with the invention for determining a particular “reference signal” 87 as denominated in FIG. 8. FIG. 9 represents what might be alternatively referred to as a ‘set-up’ or a ‘calibration’ process 150. An operator at the job-site fetches or acquires a sample piece of the pipe(s) to-be-welded. The object is to determine what signal the un-scraped (or un-skinned or otherwise un-cleaned) pipe provides under local conditions. Local conditions include color and type of pipe to-be-welded as well as the ambient light (in spite of shielding or hooded-enclosures to block out ambient light). Preferably this calibration or set-up cycle would likewise be logged by the data-recorder 100 for audit purposes F101 to determine irregularities and the like.
Step one A160 involves the operator procuring a sample of the un-scraped (or un-skinned or insufficiently cleaned) pipe of the color and type to-be-welded before the welding process(es) are to be attempted. It is preferred if this step is done often. For example, a work day which will involve a lot of welding of the same type and color of pipe deserves calibration at least at the beginning of the day. Indeed the calibration process 150 might best be performed several times during a day as there are likely changing circumstances with the quality of the pipe or else the amount of leakage of ambient light. In contrast, with reference to FIG. 6, the diminishment of the received signal 83 as compared to a reference 87 of un-scraped (or un-skinned or insufficiently cleaned) pipe against scraped (or its corollary sufficiently skinned or cleaned) pipe is ordinarily substantial:—particularly for yellow and white pipe, yellow pipe being more common in natural gas piping.
A succeeding step A170 involves inserting one or more samples of un-scraped (or insufficiently skinned or cleaned) pipe under the probes 110 to obtain A190 a reference value 87 or {87}. Perhaps one sample is sufficient to obtain the reference value. Better yet is if the operator subjects several samples to the work of the probes 110 to provide several individual reference values 87, and with which the processor 100's control circuitry analyzes for determining a ‘statistical’ reference value {87}. FIG. 9 shows a manual way A180 of determining individual reference values 87, as by an operator manually tuning a dial as to a variable resistor (or potentiometer) or the like until such activity A190 finds a given level of diminishment of the received signal 83 in comparison to the emitted signal. The foregoing assumes the circuitry 100 is measuring signal strength.
Ultimately, by means of the foregoing, the operator establishes a reference value 87 which compares favorably to what un-scraped (or insufficiently skinned or cleaned) pipe 20 looks like.
FIG. 10 is a flowchart showing a further methodology 200 in accordance with the invention for determining F100 passing or failing pipe surface quality preceding electrofusion welding. The presumptive input or starting materials (and apparatus) include an electrofusion processor EP100 or probe-operating/signal-processing system 100 in accordance with the invention, a fitting 50 and one or more pipes 20 depending on whether it is a single pipe to-be-welded to (eg, in cases of a tapping-tee fitting 51) or more (eg., in cases of a coupling fitting 52). Step one A210 preferably comprises the original attempt to satisfactorily scrape (or skin or clean) the involved pipe section(s) prior to welding. Step two A220 presumptively comprises assembling the fitting where it belongs. The succeeding steps A230 comprise variously inputting to the electrofusion processor the particulars of the particular fitting:—nowadays that being most popularly accomplished by bar-code coding affixed to the fitting in combination with equipping the electrofusion processor with a bar-code reader (eg., “W” in FIG. 7). It is presumed that the fitting's welding particulars will be a relevant factor in surface-analysis evaluation, but then perhaps not. What is presumptively most relevant is whether the relevant pipe section(s) has(have) been properly scraped (or otherwise skinned or cleaned).
Provided that the fitting 50 is properly disposed on the presumptively-properly scraped (or skinned or cleaned) pipe section(s) 25, a preferred succeeding step A230 is to energize the probe(s). It is preferred that the electrofusion processor EP100 be disabled A120 from providing welding-power to the fitting 50's terminals unless as a condition precedent the electrofusion processor is enabled to do so by the probe control circuitry. Therefore, energizing the probes 110 for the first time affords the first opportunity to get an “operative” feedback signal 89. In contrast, if a “fail” (or “abort” or “disable”) feedback signal is obtained, the operator is faced with several choices A240. Perhaps the fitting was improperly aligned over properly scraped (or skinned or cleaned) pipe section. Re-alignment might solve the problem. Perhaps otherwise, the pipe section(s) is(are) indeed insufficiently scraped (or skinned or cleaned), and therefor the operator's only practical choice for remedy is to disassemble and re-clean (eg., scrape or skin) the involved pipe section as whole.
Such is done iteratively until ultimately a “pass” (or the like) signal 89 is obtained from the probe(s) 110's processing/control circuitry 100. Given satisfaction of the foregoing condition(s), the probe(s) 110's processing/control circuitry 100 enables (eg., no longer aborts or disables) the electrofusion processor EP100's weld functions F250 (eg., the power-supply feed to the terminals). Therefore a better likelihood of a satisfactory weld in accordance with OEM prescriptions is much more likely obtained. The invention offers the prospect of negating human error better than nowadays achieved by previously practiced practices in the field of electrofusion of thermoplastics.
FIG. 11 is sectional view comparable to FIG. 4 except showing successful completion of electrofusion welding 99 of the pipe ends 22 and coupling 52. It is an object of the invention to promote a better likelihood of achieving satisfactory welds by a machine “checking” of the condition of things precedent before welding is attempted, as well as by providing a data log of such, for auditing purposes, not as much for back-tracking to identify operators lacking integrity but more for the benign purpose of reminding operators persistently that there is log of their operations. To be abstract for a moment, a popular definition of integrity is not only that one would do as one would want for themselves but alternatively that one would “do” with the thought that someone else is watching over one's shoulder. Every action will be public, or at least exposed in the end. The data logging functions of the invention promote the concept of that “someone” else is indeed watching over one's shoulder. It's not so much an object of the invention to create an onerous “big brother,” but that given good people who work as operators, who are nevertheless pressured by productivity pressures, better it is to promote good work ethics for the larger good of public welfare or safety than to rush a job and endanger such for sake of meeting productivity targets. Given that many of the many of these electrofusion welds are made in natural gas pipelines, the stakes are paramount. It is not so much a matter of assuring no contractor forsakes its/his responsibility but that no contractor endangers the public needlessly beyond what are locally-stated or more broadly-codified acceptable criteria for constructing electrofusion-formed piping systems.
The invention having been disclosed in connection with the foregoing variations and examples, additional variations will now be apparent to persons skilled in the art. The invention is not intended to be limited to the variations specifically mentioned, and accordingly reference should be made to the appended claims rather than the foregoing discussion of preferred examples, to assess the scope of the invention in which exclusive rights are claimed.
1. A method comprising a surface-analysis determination precedent to electrofusion welding, in which a pipe or pipes to-welded to an electrofusion fitting are prescribed to meet a passing surface-quality condition, comprising the steps of:
supplying an electrofusion fitting and an electrofusion processor for completing electrofusion welding of said electrofusion fitting to an applicable section of pipe stock if such is passable for the purpose;
providing at least one signal-outputting device for inspecting at least a portion of the applicable section of the pipe stock contemporaneously prior to operation of the electrofusion processor;
feeding the output of the at least one signal-outputting device to control circuitry to determine alternately a “pass” condition which enables operation of the electrofusion processor, and hence welding, or alternatively disables operation of the electrofusion processor so that presumptively an operator would disassemble and then re-assemble the at least one signal-outputting device or fitting or both for a successive measurement, whereby during the interim the operator is afforded opportunity to skin, scrape or otherwise clean the applicable pipe section in order to obtain a “pass” condition.
2. The method of claim 1 wherein said signal-outputting device comprises a non-contact probe.
3. The method of claim 1 wherein said signal-outputting device comprises an emitter of an analysis signal and a detector of the reflection of such off the at least a portion of the applicable section of the pipe stock, said output of said signal-outputting device being a product at least in part of the detected reflection of the analysis signal.
4. Apparatus for making a surface-analysis determination precedent to electrofusion welding, in which a pipe or pipes to-welded to an electrofusion fitting are prescribed to meet a passing surface-quality condition, comprising the steps of:
control circuitry and memory for linking to an electrofusion processor that completes an electrofusion welding operation between an electrofusion fitting to an applicable section of pipe stock if such is passable for the purpose; and
at least one signal-outputting device for inspecting at least a portion of the applicable section of the pipe stock contemporaneously prior to operation of the electrofusion processor, the at least one signal-outputting device having an output to feed to the control circuitry from which the control circuitry determines alternately a “pass” condition and consequently enable operation of the electrofusion processor, and hence welding, or alternatively disables operation of the electrofusion processor so that presumptively an operator would disassemble and then re-assemble the at least one signal-outputting device or fitting or both for a successive measurement, whereby during the interim the operator is afforded opportunity to skin, scrape or otherwise clean the applicable pipe section in order to obtain a “pass” condition.
5. The apparatus of claim 4 wherein said signal-outputting device comprises a non-contact probe.
6. The apparatus of claim 4 wherein said signal-outputting device comprises an emitter of an analysis signal and a detector of the reflection of such off the at least a portion of the applicable section of the pipe stock, said output of said signal-outputting device being a product at least in part of the detected reflection of the analysis signal.
7. An electrofusion processor comprising apparatus according to claim 4.
8. A method comprising a surface-analysis determination precedent to electrofusion welding, in which a pipe or pipes to-welded to an electrofusion fitting are prescribed to meet a passing surface-quality condition, comprising the steps of:
supplying an electrofusion fitting and an electrofusion processor for completing electrofusion welding of said electrofusion fitting to an applicable section of pipe stock;
providing at least one signal-outputting device for inspecting at least a portion of the applicable section of the pipe stock contemporaneously prior to operation of the electrofusion processor;
feeding the output of the at least one signal-outputting device to control circuitry to determine alternately a “pass” condition or not, and consequently provide an operator with an indication of which as well as store the determination results to memory for future audit purposes, whereby the absence of a “pass” indication affords the operator opportunity to postpone the electrofusion welding operation as for presumptively disassembling and then re-assembling the at least one signal-outputting device or fitting or both for a successive measurement so that during the interim the operator might skin, scrape or otherwise clean the applicable pipe section in order to obtain a “pass” condition.
9. The method of claim 8 further comprising, before the activity of inspecting at least a portion of the applicable section of the pipe stock contemporaneously prior to operation of the electrofusion processor, a calibration process; said calibration process comprising the steps of:
arranging the at least one signal-outputting device to inspect a raw, or not-skinned in recent times, sample or patch of the pipe stock;
establishing with the control circuitry that the output therefrom corresponds to a calibration output; and
storing the calibration output to memory for future audit purposes.
10. The method of claim 8 wherein said electrofusion fitting bears a bar code and said electrofusion processor provides bar-code reading capability for associating specific operational instructions applicable to the electrofusion fitting according to the bar code thereof, said method further comprising storing the bar-code reading of the electrofusion fitting to memory for future audit purposes.
11. The method of claim 8 wherein said electrofusion processor requires input of the electrofusion fitting's identity in order to associate specific operational instructions applicable thereto, or requires input of specific operational instructions applicable to the electrofusion fitting's identity, said method further comprising storing said input to memory for future audit purposes.
12. The method of claim 8 wherein said signal-outputting device comprises a non-contact probe.
13. The method of claim 8 wherein said signal-outputting device comprises an emitter of an analysis signal and a detector of the reflection of such off the at least a portion of the applicable section of the pipe stock, said output of said signal-outputting device being a product at least in part of the detected reflection of the analysis signal.
14. Apparatus for making a surface-analysis determination precedent to electrofusion welding, in which a pipe or pipes to-welded to an electrofusion fitting are prescribed to meet a passing surface-quality condition, comprising the steps of:
control circuitry and memory for linking to an electrofusion processor that completes an electrofusion welding operation between an electrofusion fitting to an applicable section of pipe stock if such is passable for the purpose; and
at least one signal-outputting device for inspecting at least a portion of the applicable section of the pipe stock contemporaneously prior to operation of the electrofusion processor, the at least one signal-outputting device having an output to feed to the control circuitry from which the control circuitry determines alternately a “pass” condition or not, and consequently provides an operator with an indication of which as well as store the determination results to memory for future audit purposes, whereby the absence of a “pass” indication affords the operator opportunity to postpone the electrofusion welding operation as for presumptively disassembling and then re-assembling the at least one signal-outputting device or fitting or both for a successive measurement so that during the interim the operator might skin, scrape or otherwise clean the applicable pipe section in order to obtain a “pass” condition.
15. The apparatus of claim 14 wherein the control circuitry is further configured for storing to memory the output of a calibration process that comprises arranging the at least one signal-outputting device to inspect a raw, or not-skinned in recent times, sample or patch of the pipe stock; establishing with the control circuitry that the output therefrom corresponds to a calibration output; and storing the calibration output to memory for future audit purposes.
16. An electrofusion processor comprising apparatus according to claim 14.
17. The electrofusion processor of claim 16 further comprising a bar-code reader for reading bar codes on electrofusion fittings in order to associate specific operational instructions applicable thereto as according to the bar code thereon, said electrofusion processor being further configured for storing the bar-code reading of the electrofusion fitting to memory for future audit purposes.
18. The electrofusion processor of claim 16 being configured for input of the electrofusion fitting's identity in order to associate specific operational instructions applicable thereto, or input of specific operational instructions applicable to the electrofusion fitting's identity, said electrofusion processor being further configured for storing said input to memory for future audit purposes.
19. The apparatus of claim 14 wherein said signal-outputting device comprises a non-contact probe.
20. The apparatus of claim 14 wherein said signal-outputting device comprises an emitter of an analysis signal and a detector of the reflection of such off the at least a portion of the applicable section of the pipe stock, said output of said signal-outputting device being a product at least in part of the detected reflection of the analysis signal.