2016-05-03
14/731,227
2015-06-04
US 9,330,902 B1
2016-05-03
-
-
Jami M Valentine
J.C. Patents
2035-06-04
Smart Summary: A new method creates a HfOx film using a process called atomic layer deposition (ALD). First, a substrate is prepared, and the ALD process is divided into several stages. Each stage involves applying two materials, HfCl4 and H2O, in varying amounts to build the film layer by layer. The ratio of HfCl4 to H2O increases with each stage to enhance the film's properties. This approach helps produce a thin, high-quality insulating layer for semiconductor devices like transistors. π TL;DR
A method for forming a HfOx film based on atomic layer deposition (ALD) process includes: providing a substrate; dividing a plurality of ALD cycles as needed into multiple depositing stages, wherein each of the ALD cycles includes applying HfCl4 pulse and applying H2O pulse over the substrate and a content ratio of HfCl4 to H2O is different and increasing for the depositing stages; and performing the depositing stages to form a HfOx film.
Get notified when new applications in this technology area are published.
H01L29/517 » CPC further
Semiconductor devices adapted for rectifying, amplifying, oscillating or switching, or capacitors or resistors with at least one potential-jump barrier or surface barrier, e.g. PN junction depletion layer or carrier concentration layer; Details of semiconductor bodies or of electrodes thereof; Multistep manufacturing processes therefor; Electrodes ; Multistep manufacturing processes therefor characterised by the materials of which they are formed; Metal-insulator-semiconductor electrodes, e.g. gates of MOSFET; Insulating materials associated therewith the insulating material comprising a metallic compound, e.g. metal oxide, metal silicate
H01L21/3205 IPC
Processes or apparatus adapted for the manufacture or treatment of semiconductor or solid state devices or of parts thereof; Manufacture or treatment of semiconductor devices or of parts thereof the devices having at least one potential-jump barrier or surface barrier, e.g. PN junction, depletion layer or carrier concentration layer the devices having semiconductor bodies comprising elements of Group IV of the Periodic System or AB compounds with or without impurities, e.g. doping materials; Treatment of semiconductor bodies using processes or apparatus not provided for in groups Β -Β to form insulating layers thereon, e.g. for masking or by using photolithographic techniques ; After treatment of these layers; Selection of materials for these layers Deposition of non-insulating-, e.g. conductive- or resistive-, layers on insulating layers; After-treatment of these layers
H01L21/02 IPC
Processes or apparatus adapted for the manufacture or treatment of semiconductor or solid state devices or of parts thereof Manufacture or treatment of semiconductor devices or of parts thereof
H01L29/66 IPC
Semiconductor devices adapted for rectifying, amplifying, oscillating or switching, or capacitors or resistors with at least one potential-jump barrier or surface barrier, e.g. PN junction depletion layer or carrier concentration layer; Details of semiconductor bodies or of electrodes thereof; Multistep manufacturing processes therefor Types of semiconductor device ; Multistep manufacturing processes therefor
H01L29/51 IPC
Semiconductor devices adapted for rectifying, amplifying, oscillating or switching, or capacitors or resistors with at least one potential-jump barrier or surface barrier, e.g. PN junction depletion layer or carrier concentration layer; Details of semiconductor bodies or of electrodes thereof; Multistep manufacturing processes therefor; Electrodes ; Multistep manufacturing processes therefor characterised by the materials of which they are formed; Metal-insulator-semiconductor electrodes, e.g. gates of MOSFET Insulating materials associated therewith
H01L21/28 IPC
Processes or apparatus adapted for the manufacture or treatment of semiconductor or solid state devices or of parts thereof; Manufacture or treatment of semiconductor devices or of parts thereof the devices having at least one potential-jump barrier or surface barrier, e.g. PN junction, depletion layer or carrier concentration layer the devices having semiconductor bodies comprising elements of Group IV of the Periodic System or AB compounds with or without impurities, e.g. doping materials Manufacture of electrodes on semiconductor bodies using processes or apparatus not provided for in groups -
1. Field of Invention
The present invention relates to a semiconductor process, and more particularly to a method for forming HfOx film based on atomic layer deposition (ALD) process.
2. Description of Related Art
MOS is a basic structure widely applied to various semiconductor devices, such as memory devices, image sensors and display devices. An electric device is required to be made lighter, thinner and smaller, in which that MOS transistor needs to be scaled down accordingly. In order to assure the function of MOS transistor is in well performance, a rather thin layer of high-K material, such as HfOx film, is used to serve as a gate insulating layer in the transistor.
The traditional manner to form the HfOx film is based on ALD process, in which each ALD cycle just forms a layer with the thickness of atomic order, such as 0.5 or 0.6 Angstroms. After a number of ALD cycles, an intended thickness of the HfOx film can be formed.
FIG. 1 is a drawing, schematically illustrating a traditional apparatus form forming the HFOx film. In FIG. 1, the traditional apparatus may include a holder 52, which can hold a substrate 54, such as silicon substrate. The substrate 54 is located inside a chamber 50. The chamber has an inlet and outlet, so the material of H2O and HfCl4 can be applied through the chamber 50 by a form of pulses. Due to the reaction between H2O and HfCl4, the HfOx film can be formed. Here, the index x of HfOx ideally is 2. However, the index x for this stage of formation is usually not exactly equal to 2, as usually known in the art.
FIG. 2 is a drawing, schematically illustrating a traditional ALD cycles to form the HFOx. For one ALD cycle, a H2O pulse with pulse time oft may be applied in to the chamber 50 and then a HfCl4 pulse with pulse time oft may be applied after the H2O pulse. The material of HfCl4 may react with the H2O staying on the substrate, so an atomic layer of HfOx can be formed. After a certain number of ALD cycles, the HfOx film with intended thickness can be formed.
The present invention provides a method for forming HfOx film based on ALD process, in which a ratio of Hf to O in the HfOx film can be in better uniformity with respect to the depth of the HfOx film.
The present invention provides a method for forming a HfOx film based on ALD process comprising: providing a substrate; dividing a plurality of ALD cycles as needed into multiple depositing stages, wherein each of the ALD cycles comprises applying HfCl4 pulse and applying H2O pulse over the substrate and a content ratio of HfCl4 to H2O is different and increasing for the depositing stages; and performing the depositing stages to form a HfOx film.
According to an embodiment of the present invention, the substrate is silicon substrate.
According to an embodiment of the present invention, a range of the content ratio of HfCl4 to H2O for a first stage of the depositing stages is 0.1 to 2.
According to an embodiment of the present invention, a range of the content ratio of HfCl4 to H2O for a second stage of the depositing stages is 0.2 to 2.
According to an embodiment of the present invention, a range of the content ratio of HfCl4 to H2O for a third stage of the depositing stages is 0.3 to 2.
According to an embodiment of the present invention, a range of the content ratio of HfCl4 to H2O for a fourth stage of the depositing stages is 0.4 to 2 and a range of the content ratio of HfCl4 to H2O for a fifth stage of the depositing stages is 0.5 to 2.
According to an embodiment of the present invention, the method further comprises: performing at least a subsequent processing step over the HfOx film to increase a dielectric constant of the HfOx film; and forming a metal gate over the HfOx film.
According to an embodiment of the present invention, in the step of applying the H2O pulse, O2 and O3 are involved.
According to an embodiment of the present invention, each of the ALD cycle over the substrate comprises: the step of applying H2O pulse, with a first pulse time; purging H2O; the step of applying HfCl4 pulse, with a second pulse time; purging HfCl4, wherein a ratio of the second pulse time to the first pulse time is accordingly changed with respect to the depositing stages.
According to an embodiment of the present invention, additional steps of applying H2O pulse and purging H2O are performed after the depositing stages.
According to an embodiment of the present invention, a gate structure can be formed on the HfOx film.
According to an embodiment of the present invention, the step of forming the gate structure comprises foil ing a dummy gate stack and further comprises performing a metal gate replacement process for replacing the dummy gate stack with a metal gate structure.
In view of the above, the HfOx film can be formed in multiple stages with different ratio of HfCl4 to H2O and can have better uniformity of the Hf/O ratio with respect to the depth of the HfOx film.
In order to make the aforementioned and other objects, features and advantages of the present invention comprehensible, a preferred embodiment accompanied with figures is described in detail below.
The accompanying drawings are included to provide a further understanding of the invention, and are incorporated in and constitute a part of this specification. The drawings illustrate embodiments of the invention and, together with the description, serve to explain the principles of the invention.
FIG. 1 is a drawing, schematically illustrating a traditional apparatus form forming the HfOx film.
FIG. 2 is a drawing, schematically illustrating a traditional ALD cycles to form the HFOx.
FIG. 3 is a drawing, schematically illustrating a mechanism for applying the H2O pulses and the HfCl4 pulses within ALD cycles, according to an embodiment of the present invention.
FIG. 4 is a drawing, schematically illustrating a mechanism for ALD cycle of H2O pulses and HfCl4 pulses to form the atomic layer of HfOx, according to an embodiment of the present invention.
FIG. 5 is a drawing, schematically illustrating a ratio of Hf to O in the HfOx film with respect to the number of ALD cycles applied, according to an embodiment of the present invention.
FIG. 6 is a drawing, schematically illustrating the changes of the ratios of HfCl4 pulses to H2O pulses in different stages, according to an embodiment of the present invention.
FIGS. 7A-7D are drawings, schematically illustrating a process for forming a metal gate on the HfOx film, according to an embodiment of the present invention.
Reference will now be made in detail to the present preferred embodiments of the invention, examples of which are illustrated in the accompanying drawings. Wherever possible, the same reference numbers are used in the drawings and the description to refer to the same or like parts.
The HfOx film has high dielectric constant (K) and can be used to serve as the gate insulating layer, which is required to be thin for the MOS transistor with reduced size. The HfOx film can be formed based on ALD process, in which the thickness is determined by the number of ALD cycles being applied.
Usually, after the HfOx film is preliminarily formed, the index x of the chemical form is not exactly equal to 2 as HfO2. So, at least a subsequent processing step over the HfOx film would be performed to increase the dielectric constant of the HfOx film. For example, N atoms are subsequently applied to the HfOx. However, if the Hf/O ration in the HfOx film is varying with the depth, then the result could be not good as expected because a uniform concentration of the N atoms are usually applied within the whole HfOx film.
The present invention has investigated the ratio of Hf/O in the HfOx film with respect to the depth. Indeed, the ratio of Hf/O in the HfOx film is varying with the depth. The present invention proposes that the HfOx film is formed by the ALD cycles in at least two stages, in which a content ratio of HfCl4 to H2O is different and increasing for the depositing stages.
Several embodiments are provided to describe the present invention, but the present invention is not limited to the provided embodiments.
FIG. 3 is a drawing, schematically illustrating a mechanism for applying the H2O pulses and the HfCl4 pulses within ALD cycles, according to an embodiment of the present invention. In FIG. 3, the H2O pulses are applied to the apparatus as for example shown in FIG. 1, over the substrate 54, such as silicon substrate. The pulse time in time is t1. The pulse time can also be referred as pulse width. In alternate time periods not apply the H2O pulses, the HfCl4 pulses are applied to the apparatus, in which the pulse time of the HfCl4 pulses in time is t2. The ratio of the t2 to t1 is not always a constant but different and increasing with respect to the depositing stages.
Here, the concentrations of the H2O and HfCl4 in the each pulse with respect to time is the same as in an embodiment, so the ratio of HfCl4 to H2O can be determined by the ratio of t2 to t1. However, if concentrations of the H2O and HfCl4 in the pulses are different, the pulse time t1 or t2 would be accordingly adjusted to assure the ratio of HfCl4 to H2O is achieved as given.
Further, the mechanism of ALD cycle for the HfOx film is described. FIG. 4 is a drawing, schematically illustrating a mechanism for ALD cycles of H2O pulses and HfCl4 pulses to form the atomic layer of HfOx, according to an embodiment of the present invention.
In FIG. 4, one ALD cycle may contribute a thickness, such as about 0.5, 06 Angstroms in an example, for the HfOx film. In an example, one ALD cycle may include applying H2O pulse, with a first pulse time; purging H2O; applying HfCl4 pulse, with a second pulse time; and purging HfCl4. A ratio of the second pulse time to the first pulse time is accordingly changed with respect to the depositing stages.
When applying H2O pulse over the substrate, the H2O molecules would adhere to the substrate. Then, the H2O is purged to leave a monolayer of H2O. When applying the HfCl4 pulse, the molecules of HfCl4 would react with H2O molecules. After purging the HfCl4, a monolayer of the ALD layer after reaction is formed. At this stage, one ALD cycle is done and form the monolayer with a thickness, such as one Angstrom, or alternatively 0.5-0.6 Angstroms. So, an intended thickness of the HfOx film usually needs a certain number of ALD cycles. After the HfOx film with the intended thickness is formed by the ALD cycles, additional H2O pulse may be applied again at the end stage to remove chlorine and the H2O purging step is applied also.
Before describing the control of the content ratio of HfCl4 to H2O, the present invention have investigated the ratio of Hf to O in the HfOx film with respect to the depth. FIG. 5 is a drawing, schematically illustrating a ratio of Hf to O in the HfOx film with respect to the number of ALD cycles applied, according to an embodiment of the present invention.
In FIG. 5, taking a constant ratio for Hf to O, such as about 0.6, the number of ALD cycles being applied would indicate the depth of the HfOx film in physical property. The data as investigated by the present invention shows that the Hf/O ratio is not a constant and increasing with the number of the ALD cycles. This implies that the later ALD cycle, or the shallow portion of the HfOx film, has less O content, resulting in higher ratio of Hf/O.
The present invention proposes that content ratio of HfCl4 to H2O for the ALD cycles are not kept constant but increasing instead. Under the aspect, the present invention proposes that the ALD cycles as needed to have the intended thickness can be divided into at least two depositing stages, in which the content ratio of HfCl4 to H2O is increasing. FIG. 6 is a drawing, schematically illustrating the changes of the ratios of HfCl4 pulses to H2O pulses in different stages, according to an embodiment of the present invention.
To form the HfOx film, it usually needs a large number of ALD cycles. In practical strategy, the ALD cycles can be divided into multiple depositing stages. In an example, five depositing stages as an example is provided for describing the present invention. Each depositing stage includes multiple ALD cycles, such as 5-10 cycles. However, depending on the intended thickness of the whole HfOx film, the number of depositing stages can be 3 stages, 2-5 stages or even more.
In the example, the content ratio of HfCl4 to H2O for the first depositing stage can be in a range of 0.1 to 2. The content ratio in the example is 0.1. The first depositing stage contributes a part of the intended thickness, which is at the bottom portion of the HfOx film. The second depositing stage has the content ratio of HfCl4 to H2O in a range of 0.2 to 2 as an example, and is the greater than that in the first depositing stage. The content ratio in the example is 0.2. Likewise, the third depositing stage has the content ratio of HfCl4 to H2O in a range of 0.3 to 2 as an example, and is the greater than that in the second depositing stage. The content ratio in the example is 0.3. The fourth depositing stage has the content ratio of HfCl4 to H2O in a range of 0.4 to 2 as an example, and is the greater than that in the third depositing stage. The content ratio in the example is 0.4. The fifth depositing stage has the content ratio of HfCl4 to H2O in a range of 0.5 to 2 as an example, and is the greater than that in the fourth depositing stage. The content ratio in the example is 0.5.
Due to the effect as shown in FIG. 5, the later depositing stage has larger O content or less Hf content. This ratio of Hf to O in the HfOx film may approach to a better uniformity in all depth, about remaining at the beginning level of the first depositing stage.
Further, the HfOx film belongs to a dielectric material having high dielectric constant, so HfOx film is also a good candidate for serving as the gate insulating layer in the MOS transistor. An example in application for forming a metal gate of transistor is described as follows.
FIGS. 7A-7D are drawings, schematically illustrating a process for forming a metal gate on the HfOx film, according to an embodiment of the present invention. In FIG. 7A, a substrate 300 is provided. The substrate 300 is silicon substrate in an example. Isolation structures 302 are formed in the substrate 300 to define a device region. A HfOx layer 510, serving as a high-K layer, is formed on the substrate 300 based on ALD process as previously described. The HfOx layer 510 can be performed with further subsequent process to increase the dielectric constant, such as applying N atoms into the HfOx layer 510. A dummy gate 511, such as polysilicon gate, is staked on the HfOx layer 510. A cap layer 512 is formed on the dummy gate 511. The dummy gate structure 304 is then formed from the HfOx layer 510, the dummy gate 511 and the cap layer 512 in the example.
In 7B, a spacer 514 is formed on sidewalls of the dummy gate structure 304. The lightly doped region 504β² and heavily doped region 504 are also formed in the substrate 300. A contact etch stop layer 310 is formed over the substrate 300. An inter-layer dielectric (ILD) layer 312 is formed on the contact etch stop layer 310.
In FIG. 7C, a chemical mechanical polishing process in an example is performed to polish the ILD layer 312, the contact etch stop layer 310, the spacer 514 and the cap layer 512, until the dummy gate 511 is exposed. Then, the dummy gate 511 of polysilicon material is etched away to expose the HfOx layer 510 and the spacer 514. Then, a space 516, originally occupied by the dummy gate 511, is formed.
In FIG. 7D, a work function metal layer 518 is formed over the substrate 300, being conformal to the surface structure at top. A low resistance metal layer 520 is formed over the work function metal layer 518 and fully fills into the space 516. Another polishing process is performed again until the ILD layer 312 is exposed. The metal gate 522 is formed, including the work function metal layer 518 and the low resistance metal layer 520 in the example. The processes in FIGS. 7A-7D can be generally referred as a metal gate replacement process.
The metal gate 522 is indeed formed on the HfOx layer 510, which is formed by the method of the present invention. The gate current leak can be reduced and gate reliability can be improved.
The present invention has proposed the method for forming a HfOx film based ALD process includes: providing a substrate; dividing a plurality of ALD cycles as needed into multiple depositing stages, wherein each of the ALD cycles includes applying HfCl4 pulse and applying H2O pulse over the substrate and a content ratio of HfCl4 to H2O is different and increasing for the depositing stages; and performing the depositing stages to form a HfOx film.
The present invention has been disclosed above in the preferred embodiments, but is not limited to those. It is known to persons skilled in the art that some modifications and innovations may be made without departing from the spirit and scope of the present invention. Therefore, the scope of the present invention should be defined by the following claims.
1. A method for forming a HfOx film based on atomic layer deposition (ALD) process, comprising:
providing a substrate;
dividing a plurality of ALD cycles as needed into multiple depositing stages, wherein each of the ALD cycles comprises applying HfCl4 pulse and applying H2O pulse over the substrate and a content ratio of HfCl4 to H2O is different and increasing for the depositing stages; and
performing the depositing stages to form a HfOx film.
2. The method of claim 1, wherein the substrate is silicon substrate.
3. The method of claim 1, wherein a range of the content ratio of HfCl4 to H2O for a first stage of the depositing stages is 0.1 to 2.
4. The method of claim 3, wherein a range of the content ratio of HfCl4 to H2O for a second stage of the depositing stages is 0.2 to 2, a range of the content ratio of HfCl4 to H2O for a third stage of the depositing stages is 0.3 to 2.
5. The method of claim 4, wherein a range of the content ratio of HfCl4 to H2O for a third stage of the depositing stages is 0.3 to 2.
6. The method of claim 5, wherein a range of the content ratio of HfCl4 to H2O for a fourth stage of the depositing stages is 0.4 to 2 and a range of the content ratio of HfCl4 to H2O for a fifth stage of the depositing stages is 0.5 to 2.
7. The method of claim 1, further comprising:
performing at least a subsequent processing step over the HfOx film to increase a dielectric constant of the HfOx film; and
forming a metal gate over the HfOx film.
8. The method of claim 1, wherein in the step of applying the H2O pulse, O2 and O3 are involved.
9. The method of claim 1, wherein each of the ALD cycle over the substrate comprises:
the step of applying H2O pulse, with a first pulse time;
purging H2O;
the step of applying HfCl4 pulse, with a second pulse time;
purging HfCl4,
wherein a ratio of the second pulse time to the first pulse time is accordingly changed with respect to the depositing stages.
10. The method of claim 9, wherein additional steps of applying H2O pulse and purging H2O are performed after the depositing stages.
11. The method of claim 1, wherein the x in HfOx is in a range between 0.8 and 1.7.
12. The method of claim 1, further comprising forming a gate structure on the HfOx film.
13. The method of claim 12, wherein the step of forming the gate structure comprises:
forming a dummy gate stack on the HfOx film; and